Hamada Rust (Temmoku)


Hamada Rust cone 10

77.0 Custer Feldspar
0.1 Silica
6.2 Whiting
4.3 Kaolin
12.4 Gerstley Borate
7.5 Red Iron Oxide

Procelain, thrown and altered, cone 10 reduction.


John Britt
www.johnbrittpottery.com/wks.htm